Cracking simulation and analysis of the mortise-and-tenon wet joints in Precast reinforced concrete ribbed girder Bridges

Zhang, Xiaotao; Tian, Shuai*; Zhang, Suhe; Sun, Bo
Science Citation Index Expanded
-

摘要

Flexural tests were conducted on the normal section of two different forms of specimens with wet joints to study the damage and cracks of mortise-and-tenon wet joints. Simulations were performed to analyze the mortise-and-tenon joint specimens. The extent of damage and development of cracks of specimens with straight joints and mortise-and-tenon joints are similar. The interface cracking of the specimens with mortise-and-tenon joints is often caused by concrete cracking at the root. Different tenon sizes have a negligible effect on the cracking load and overall bearing capacity of specimens. Therefore, the tenon end and depth sizes are considered 25-37.5% of the joint width, and the transition zone of the joint interface is selected to be 100-150 mm. According to the calculation formula of the flexural bearing capacity at the wet joint position and reduction factor of straight joints phi(f), the correction coefficient of mortise-and-tenon joints phi(s)was proposed to be 1.03.

关键词

Ribbed girder bridge wet joints mortise and tenon form flexural load capacity numerical simulation